#TheBatteryShow

Venue: Goyang·South Korea

K-BATTERY SHOW 2025

Update: September 10, 2025
K-BATTERY SHOW 2025-NEWARE

The New K-BATTERY SHOW for the Coming Future !

The secondary battery materials, parts, and equipment exhibition (K-BATTERY SHOW), is an exhibition represented the secondary battery industry that will lead the fourth industrial revolution through with future technological IT convergence such as the Internet of Things and artificial intelligence. K-BATTERY SHOW will be held concurrently with and H2MEET SHOW and can create synergistic effects.

Secondary Battery is a key element of Electrification and Cordless tools for the future

Electrification and Cordless tools are the core element for the future of industries. It brings in a new era which all things are powered by second batteries.
All efforts should be made on digital transformation and eco-friendliness for a sustainable future which needed to improve industrial ecosystems.

Learn more>


NEWARE TECHNOLOGY LIMITED

1314 ,Gasan Digital 2-ro 70, Geumcheon-gu, Seoul 19th Taerung Techno Town, Gasan-dong, Geumcheon-gu, Seoul , Korea 08589

neware-battery-test-newareAI neware-battery-test-newareStore neware-battery-test-neware-newell


· Popular Product


NEWARE-Battery Tester-CT-8002Q-5V100mA

Battery Test Equipment-NEWARE

CT-8002Q-5V100mA-124

CT-8000 Battery Testing System

● Voltage&Current Accuracy:±0.01% F.S.

● Recording Frequency:100Hz

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test:1GB/CH

● Cycle Life, GITT Test, DCIR Test, dQ/dV Curve

NEWARE-Battery Tester-CT-4008Q-5V100mA-124

Battery Test Equipment-NEWARE

CT-4008Q-5V100mA-124

CT-4000 Battery Testing System

● Voltage & Current Accuracy:±0.01% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test: 1GB


CE-4008Q-5V15A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V15A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

Bttery test equipment-NEWARE-CE-4008Q-5V20A-Battery Testing System

Battery Test Equipment-NEWARE

CE-4008Q-5V20A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

CE-4008Q-5V30A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V30A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

NEWARE-Battery Tester-CE-5012-5V600A

Battery Test Equipment-NEWARE

CE-5012-5V600A

CE-5000 Battery Testing System

● Voltage Accuracy:±0.02% F.S.

● Current Accuracy:±0.05% F.S.

● Resolution Ratio AD/DA:16bit

● Current Response Time:≤1ms

● Minimum Pulse Width:100ms

● Off-Line Test:1GB/CH

NEWARE-Battery Tester-CE-6000 Cell Testing System

Battery Test Equipment-NEWARE

CE-6000 Cell Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:100Hz

● Current Conversion Time:≤6ms

● Current Response Time:≤3ms

● Minimum Pulse Width:100ms

● Feedback Efficiency (Max) :75%

NEWARE-Battery Teste-CT-9002-5V6A-F-204n

Battery Test Equipment-NEWARE

CT-9002-5V6A-F-204n

CT-9000 Battery Testing System

● Voltage & Current Accuracy:±0.02% F.S.

● Voltage & Current Stability:±0.01% F.S.

● Recording Frequency:1000Hz

● Resolution AD:16bit

● Current Response Time:≤100μs

● Off-Line Test: 1GB

NEWARE and Cookies
We use Cookie to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.