Features

Tech Specs

Resources

Interpreting the beauty of research with data.

59℉~140℉<br>(15℃~60℃ )
Temperature Range
59℉~140℉
(15℃~60℃ )
16CH
Number of Channels
16CH
≤1.8℉(1℃)(No load and stable temperature)
Temperature Fluctuation
≤1.8℉(1℃)(No load and stable temperature)
77℉ ~ 140℉≤50min<br>(25℃~60 ℃)
Heating Efficiency
77℉ ~ 140℉≤50min
(25℃~60 ℃)
77℉ ~ 59℉≤60min<br>(25℃~15 ℃)
Cooling Efficiency
77℉ ~ 59℉≤60min
(25℃~15 ℃)
±3.6℉(±2.0℃)(No load and stable temperature)
Temperature Deviation
±3.6℉(±2.0℃)(No load and stable temperature)

WHW-25L-S Mini Constant Temperature Chamber compresses experimental capabilities to the extreme. Despite its compact size, it possesses powerful experimental functions. Whether you are conducting research and testing in a laboratory, studio, or office desk, this mini constant temperature test chamber can provide you with professional-level temperature control and stability.


All-around product tour.

Refined temperature control for long-lasting insulation.

A 40mm thick polyurethane foam layer is installed between the outer cold-pressed steel plate and the inner stainless steel plate, providing superior internal temperature protection to ensure more accurate and reliable data.

A 40mm thick polyurethane foam layer is installed between the outer cold-pressed steel plate and the inner stainless steel plate, providing superior internal temperature protection to ensure more accurate and reliable data

Neatly organized: 16 testing channels.

With a compact and slender body, it is more suitable for small-scale development and experiments. It has a practical volume of 25L and occupies less than 5.38sq.ft of space, freeing up more desktop space. It allows for real-time observation of experimental conditions inside the chamber. The high-quality insulated battery cell tray can accommodate up to 16 coin battery cells.

NEWARE-WHW-25 Constant Temperature Chamber can accommodate a maximum of 16 button batteries with a usable volume of 25L and occupies a floor space of 5.38 sq

Unified management, smooth connectivity.

The constant temperature test chamber, battery cell testing equipment, and computer are interconnected through channel wires and data communication cables to achieve hardware interconnectivity. The computer features integrated BTS (Battery Test System) for temperature control settings and battery cell testing.


constant temperature test chamber, battery cell testing equipment, and computer are interconnected through channel wires and data communication cables to achieve hardware interconnectivity. The computer features integrated BTS (Battery Test System) for temperature control settings and battery cell testing

Intuitive interface, effortless operation.

WHW-25L-S prioritizes user experience and incorporates a touch LCD screen design with a user-friendly graphical interface and flexible configuration options. It features automatic screen wake-up through infrared human body sensing within a 1.5-meter range, allowing users to easily set up and manage the device.

The NEWARE-WHW-25 Constant Temperature Chamber - battery tester features a touch LCD screen design and infrared human body induction for automatic screen wake-up function

Powerful heat dissipation for optimal stability.

According to the set temperature value, the control system automatically calculates and controls the output of the semiconductor refrigeration (heating) module using the newly developed fuzzy PID algorithm by New Wei, in order to achieve dynamic balance. 


NEWARE-WHW-25 Constant Temperature Chamber - battery tester has powerful heat dissipation capability

The axial flow fan circulates the air evenly, with a large air outlet, ensuring uniform and fast heat dissipation.


NEWARE-WHW-25 Constant Temperature Chamber - battery tester ,The axial flow fan circulates the air evenly, with a large air outlet, ensuring uniform and fast heat dissipation

Perpetual dedication to safety protection.

● Over-temperature protection 

● Electrical protection 

● Abnormal monitoring of circulating fan operation


NEWARE-WHW-25 Constant Temperature Chamber - battery tester is equipped with safety protection functions such as over-temperature protection, electrical protection, and abnormal monitoring of the circulating fan operation

· Technical Specifications

Equipment name Mini Constant Temperature Chamber
Nominal content product 25L
Inner box size W280mm × D250mm × H330mm
Overall dimensions W360mm × D450mm × H500mm
Net weight of the equipment About 40kg
Test the environmental conditions Ambient temperature is + 25℃, relative humidity is 85%, with no sample in the test box (no load)
Temperature range 15~60℃
Temperature fluctuation degree 1℃ (equivalent to ± 0.5℃, with no load and stable temperature)
Temperature deviation ± 2.0℃ (when no load and temperature is stable)
Product application Constant temperature test of buckle cell and new energy small soft package polymer cell (millipere level)
Limit the sample This test equipment is prohibited by:
· Test or storage of samples of inflammable, explosive and volatile substances
· Test or storage of test samples of corrosive substances
· Test or storage of samples of strong electromagnetic emission sources
· Test and storage of test samples of radioactive substances
· Test and storage of test samples of highly toxic substances
· Testing or storage of tests or specimens that may produce such substances or objects

Want to explore further?
Download NEWARE product technical specifications for more details.

Download

Auxilaries and Optional Accessories

To support these high-precision measurement tools, we offer a wide range of product accessories. NEWARE Store: One-stop purchasing platform.

Electrochemical Instruments

We offer powerful battery test equipments, environmental test chambers to provide comprehensive testing support for battery testing.

CE-4008Q-5V30A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V30A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

CE-4008Q-5V15A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V15A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

NEWARE-Battery Tester-CT-4008Q-5V100mA-124

Battery Test Equipment-NEWARE

CT-4008Q-5V100mA-124

CT-4000 Battery Testing System

● Voltage & Current Accuracy:±0.01% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test: 1GB


NEWARE-Battery Tester-CT-8002Q-5V100mA

Battery Test Equipment-NEWARE

CT-8002Q-5V100mA-124

CT-8000 Battery Testing System

● Voltage&Current Accuracy:±0.01% F.S.

● Recording Frequency:100Hz

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test:1GB/CH

● Cycle Life, GITT Test, DCIR Test, dQ/dV Curve

NEWARE-Battery Tester-Power Cell All-in-One-WGDW-380L-2-40BFC-5V600A8CH

NEWARE-Environmental Test Chamber

WGDW-380L-2-40BFC-5V600A8CH

Power Cell All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:100Hz

● Temperature Fluctuation:≤1.8℉(1℃)

● Temperature Range & Deviation:-40℉ ~ 302℉±3.6℉(-40℃ ~ 150℃±2.0℃)

● Heating Efficiency:68℉ ~ 302℉ ≤60min(20℃ ~ 150℃)

● Cooling Efficiency:68℉ ~ -40℉≤60min(20℃~-40℃)

NEWARE-Battery Tester-3C All-in-One Testing System-WGDW-380L-2-40BFC-5V600A8CH

NEWARE-Environmental Test Chamber

WHW-500L-5V6A80CH-380V

3C All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:100Hz

● Number of Channels:80CH

● Temperature Range & Deviation:50℉ ~ 185℉±3.6℉(10℃ ~ 85℃±2.0℃)

● Heating Efficiency:77℉ ~ 185℉ ≤40min(25℃ ~ 85℃)

● Cooling Efficiency:77℉ ~ 50℉≤40min(25℃~10 ℃)

NEWARE-Battery Tester-All-in-One Testing System-WIHW-200L-160CH-B

NEWARE-Environmental Test Chamber

WHW-200L-160CH-B

Coin Cell All-in-One Testing System

● Voltage & Current Accuracy:±0.01% F.S.

● Recording Frequency:100Hz

● Number of Channels:160CH

● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(0℃ ~ 60℃±2.0℃)

● Heating Efficiency:77℉ ~ 140℉ ≤30min(25℃ ~ 60℃)

● Cooling Efficiency:77℉ ~ 32℉≤50min(25℃~0 ℃)

NEWARE-Battery Tester- Mini All In One Testing System-WHW-25L-L-16CH

NEWARE-Environmental Test Chamber

WHW-25L-16CH

Mini All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Sampling Time:100ms

● Number of Channels:16CH

● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(15℃ ~ 60℃±2.0℃)

● Heating Efficiency:77℉ ~ 140℉≤50min(25℃ ~ 60℃)

● Cooling Efficiency:77℉ ~ 59℉≤60min(25℃~15 ℃)

NEWARE and Cookies
We use Cookie to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.