Precision monitoring:
Unlock hidden possibilities.

The voltmeter plays a crucial role in the battery testing process.

● By measuring the voltage response of the battery under different load conditions, technicians can assess the health and performance of the battery, such as capacity, internal resistance, and energy efficiency.

 Measure the open-circuit voltage of the battery to determine its state of charge.

 During the charging and discharging process of the battery, monitor the voltage in real time to ensure that the battery operates within a safe range.

NEWARE-Battery Tester-Voltmeter-CV-NW-DCQ

Experience the power of innovation
with user-friendly design.

The voltmeter not only has precise measurement capabilities but also features user-friendly design, making operation more convenient and easy to use. With a large LCD screen, intuitive user interface, and various function options, it's easy to harness the full potential of the instrument. The intuitive interface design simplifies the operation process, allowing for quick access to measurement results. The compact body and portable design make it easy to carry to any workplace.

NEWARE-Battery Tester-Voltmeter-CV-NW-DCQ

Precision measurement unleashing boundless opportunities.

Measures voltage with extremely high accuracy and precision, meeting the demands for high precision and reliability in various voltage measurement and calibration applications, providing users with high-quality voltage measurement solutions.

NEWARE-Battery Tester-Voltmeter-CV-NW-DCQ

We offer powerful battery test equipment,
environmental test chambers to provide comprehensive testing support for battery testing.

We offer powerful battery test equipment, environmental test chambers to provide comprehensive testing support for battery testing.

CE-4008Q-5V30A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V30A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

CE-4008Q-5V15A-thumb

Battery Test Equipment-NEWARE

CE-4008Q-5V15A-SR

CE-4000 Battery Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Energy Efficiency:>65%

● Off-Line Test: 1GB

NEWARE-Battery Tester-CT-4008Q-5V100mA-124

Battery Test Equipment-NEWARE

CT-4008Q-5V100mA-124

CT-4000 Battery Testing System

● Voltage & Current Accuracy:±0.01% F.S.

● Recording Frequency:10Hz

● Sampling Time:100ms

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test: 1GB


NEWARE-Battery Tester-CT-8002Q-5V100mA

Battery Test Equipment-NEWARE

CT-8002Q-5V100mA-124

CT-8000 Battery Testing System

● Voltage&Current Accuracy:±0.01% F.S.

● Recording Frequency:100Hz

● Current Response Time:≤1ms

● Minimum Pulse Width:500ms

● Off-Line Test:1GB/CH

● Cycle Life, GITT Test, DCIR Test, dQ/dV Curve

NEWARE-Battery Tester-Power Cell All-in-One-WGDW-380L-2-40BFC-5V600A8CH

NEWARE-Environmental Test Chamber

WGDW-380L-2-40BFC-5V600A8CH

Power Cell All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:100Hz

● Temperature Fluctuation:≤1.8℉(1℃)

● Temperature Range & Deviation:-40℉ ~ 302℉±3.6℉(-40℃ ~ 150℃±2.0℃)

● Heating Efficiency:68℉ ~ 302℉ ≤60min(20℃ ~ 150℃)

● Cooling Efficiency:68℉ ~ -40℉≤60min(20℃~-40℃)

NEWARE-Battery Tester-3C All-in-One Testing System-WGDW-380L-2-40BFC-5V600A8CH

NEWARE-Environmental Test Chamber

WHW-500L-5V6A80CH-380V

3C All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Recording Frequency:100Hz

● Number of Channels:80CH

● Temperature Range & Deviation:50℉ ~ 185℉±3.6℉(10℃ ~ 85℃±2.0℃)

● Heating Efficiency:77℉ ~ 185℉ ≤40min(25℃ ~ 85℃)

● Cooling Efficiency:77℉ ~ 50℉≤40min(25℃~10 ℃)

NEWARE-Battery Tester-All-in-One Testing System-WIHW-200L-160CH-B

NEWARE-Environmental Test Chamber

WHW-200L-160CH-B

Coin Cell All-in-One Testing System

● Voltage & Current Accuracy:±0.01% F.S.

● Recording Frequency:100Hz

● Number of Channels:160CH

● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(0℃ ~ 60℃±2.0℃)

● Heating Efficiency:77℉ ~ 140℉ ≤30min(25℃ ~ 60℃)

● Cooling Efficiency:77℉ ~ 32℉≤50min(25℃~0 ℃)

NEWARE-Battery Tester- Mini All In One Testing System-WHW-25L-L-16CH

NEWARE-Environmental Test Chamber

WHW-25L-16CH

Mini All-in-One Testing System

● Voltage & Current Accuracy:±0.05% F.S.

● Sampling Time:100ms

● Number of Channels:16CH

● Temperature Range & Deviation:32℉ ~ 140℉±3.6℉(15℃ ~ 60℃±2.0℃)

● Heating Efficiency:77℉ ~ 140℉≤50min(25℃ ~ 60℃)

● Cooling Efficiency:77℉ ~ 59℉≤60min(25℃~15 ℃)

NEWARE and Cookies
We use Cookie to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.