Abnormal capacity data

Why is the impact of stopping the test on battery capacity less than the impact

Latest updated: Mar 27, 2024
  • Issue description: In testing devices of the same model, the impact on capacity after a 9-hour stoppage is less than 1%, while the impact on capacity after a power outage followed by restoration is as high as 4%.

  • The device being powered off and restarted does not affect its accuracy, and therefore does not impact the capacity. However, if there is a prolonged power outage or if the power is cut during a charging or discharging step, the voltage of the battery will fluctuate. Consequently, when power is restored, it will certainly have an impact on the capacity.

  • To verify this, the same amount of time can be used to stop and then restart the device without cutting the power.


neware-battery-test-newareAI neware-battery-test-newareStore neware-battery-test-neware-newell

Latest News

Stay informed with the latest from NEWARE.

Find the Right Battery Test Equipment for Your Needs.

Application Scenarios

Trusted testing solutions for global clients.

Solid-State Battery Research - NEWARE Solid-State Battery test
Solid-State Battery Research

The lab focuses on solid-state battery research to overcome traditional lithium batteries' safety and energy density issues, supporting environmental sustainability. It develops innovative solid-state electrolytes, refines electrode materials, and investigates ion transfer and interface stability to revolutionize battery technology.

View more
Electric Vehicle Battery
Electric Vehicle Battery

The electric vehicle battery industry is rapidly developing, focusing on technological innovation, market competition, and sustainability. Research hotspots include solid-state batteries, new types of electrolytes, BMS optimization, and recycling technologies. The environmental adaptability, safety, and economic viability of batteries are key research areas, and the industry is expected to undergo more innovation and transformation.

View more
Battery Materials Research - NEWARE battery test
Battery Materials Research

We specialize in battery preparation technology research, focusing on overcoming existing energy storage challenges by innovating in electrode materials, battery chemistry, and manufacturing processes to improve performance, enhance safety, and reduce costs. Sustainability and recycling technologies for batteries are also emphasized to mitigate environmental impacts and foster the growth of green energy.

View more
Energy Storage Battery Testing Solution
Energy Storage System

To power the energy transition, the storage industry is evolving towards large-scale, high-quality development, focusing on safety, efficiency, and lifecycle value over mere price competition.

View more
NEWARE and Cookies
We use cookies to personalize and improve your experience with our website. By continuing to browse the site you are agreeing to our use of cookies.