Battery Manufacturing Terminology
The discharge capacity of a certain cycle is set as the standard, and the decay rate is obtained by comparing each subsequent cycle with the standard cycle.
Copy the steps of one channel to other channels.
The details of the selected channel.
The resistance of the battery itself.
Accumulate the capacity of continuous charge or discharge (exclude rest step) steps.
The released capacity of a battery when it is discharged from full state to the termination voltage.
The nominal capacity per unit mass/volume.
It is used to reflect the current capacity of the battery and can be expressed as percentage ratio of the current capacity and rated capacity
The percentage of released capacity by the battery to its rated capacity.
The amount of the electric charge stored in a capacitor at a specific electric potential.
The consumed time for a Battery to discharge to the termination voltage.
The cycle number before the battery capacity is reduced to a certain value under specific charge/discharge conditions
In constant current charge/discharge process, there exists astage where the voltage changes slowly/has a steady process, the corresponding voltage value is called voltage plateau.
The corresponding capacity value when the voltage reaches the set plateau voltage.
The corresponding time when the voltage reaches the set plateau voltage.
The cathode/anode material, which attends the current formation reaction (electrochemical reaction process).