The step will be cut off when the minimum temperature of the present step auxiliary channel is less than or equal to the set value.
It represents the electricity of a battery: the amount of charge stored inside the battery when it is charged under the current of 1A for 1h.
Summary data of cycle, including cycle number, charge capacity, discharge capacity, efficiency, etc.
The voltage of the final data at the end of the step.
The maximum charging voltage or minimum discharging voltage for a being tested battery.
Software installed on the computer that can be used to operate the device.
Service program installed on the computer, the client interacts with the device through the server to store the test data uploaded by the device.
The present step will be cut off when the maximum voltage of the auxiliary channel is greater than or equal to the set value.
The present step will be cut off when the minimum voltage of the auxiliary channel is less than or equal to the set value.
The present step will be cut off when the maximum temperature of the auxiliary channel is greater than or equal to the set value.
The cycle number before the battery capacity is reduced to a certain value under specific charge/discharge conditions
In constant current charge/discharge process, there exists astage where the voltage changes slowly/has a steady process, the corresponding voltage value is called voltage plateau.
The consumed time for a Battery to discharge to the termination voltage.