Accumulate the capacity of continuous charge or discharge (exclude rest step) steps.
The released capacity of a battery when it is discharged from full state to the termination voltage.
The nominal capacity per unit mass/volume.
It is used to reflect the current capacity of the battery and can be expressed as percentage ratio of the current capacity and rated capacity
The percentage of released capacity by the battery to its rated capacity.
The amount of the electric charge stored in a capacitor at a specific electric potential.
The consumed time for a Battery to discharge to the termination voltage.
The cycle number before the battery capacity is reduced to a certain value under specific charge/discharge conditions
In constant current charge/discharge process, there exists astage where the voltage changes slowly/has a steady process, the corresponding voltage value is called voltage plateau.
The corresponding capacity value when the voltage reaches the set plateau voltage.
The corresponding time when the voltage reaches the set plateau voltage.
The cathode/anode material, which attends the current formation reaction (electrochemical reaction process).
The channel will be protected when the current of the present step is greater than or equal to the set value
The channel will be protected when the current of the present step is less than or equal to the set value.
The channel will be protected when the present step voltage is greater than or equal to the value set by the upper voltage limit.
The channel will be protected when the present step voltage is less than or equal to the value set by the upper voltage limit.